Product Details
Place of Origin: China
Brand Name: SUNPRENE
Certification: ISO9001;IATF16949
Model Number: New-high performance grade
Payment & Shipping Terms
Minimum Order Quantity: 25KG
Price: CNY 35-45/KG
Packaging Details: 25kg/bag;1000kg/bag
Delivery Time: 1-30 days
Payment Terms: L/C, D/A, D/P, T/T
Supply Ability: 10000T/year
Material: |
Thermoplastic Copolyester |
Grade: |
New-high Performance Grade |
Usage: |
Parts For Vehicles;Parts For Industry;Electrical Applications;Sports Requisits;Furniture |
Feature: |
Good Strength;Flexible;resist To Oil And Acid And Base;Excellent Dynamic Mechanical Properties |
Material: |
Thermoplastic Copolyester |
Grade: |
New-high Performance Grade |
Usage: |
Parts For Vehicles;Parts For Industry;Electrical Applications;Sports Requisits;Furniture |
Feature: |
Good Strength;Flexible;resist To Oil And Acid And Base;Excellent Dynamic Mechanical Properties |
NEW-HIGH PERFORMANCE GRADE TPC-ET MATERIAL
TPC-ET materials are block copolymers consisting of a hard segment of polyester and a soft segment based on polyether or polyester.among which, polyether soft segment and non crystalline polyester comprise amorphous phase while polyester hard segment partly crystallizes to form crystal domain as physical crosslink point.
TPC-ET material combines the desirable elasticity of rubber and the strength of engineering plastics. Compared with rubber, it shows better processing properties and longer service life. The soft segment endows elasticity for TPC-ET and makes it act like rubber while the hard segment endows processing properties to make it just like plastics. In contrast to engineering plastics, TPC-ET exhibits same good strength but better flexibility and dynamic mechanical properties.
New-high performance grade SUNPRENE® TPC-ET material
Advanced technology and equipments,Optimized raw materials and formula;All improved properties upon previous high performance grade TPC-ET material for high-end applications use.
Physical Properties | Shore Hardness | Density | Tensile Strength | Elongation at Break | Flexural Modulus | Tear Strength | Melting Point | Melt Flow Index | |
Unit | HD(3S) | g/cm3 | Mpa ≥ | % ≥ | Mpa ≥ | kN·m-1 ≥ | ℃ | g/10min | |
Test Methods | ISO868 | ISO1183 | ISO527-1 | ISO527-1 | ISO178 | ISO34 | ISO3146 | ISO1133 | |
New-high performance grades | H1525 | 25 | 1.07 | 22 | 1300 | 18 | 65 | 167 | 15±3 |
H1530 | 29 | 1.08 | 27 | 1300 | 25 | 80 | 171 | 15±3 | |
H1835 | 34 | 1.10 | 32 | 1200 | 34 | 85 | 182 | 18±3 | |
H1540 | 40 | 1.12 | 38 | 1100 | 45 | 100 | 176 | 15±3 | |
H1045 | 45 | 1.14 | 40 | 1000 | 75 | 120 | 184 | 10±2 | |
H1050 | 51 | 1.19 | 46 | 900 | 140 | 130 | 198 | 10±3 | |
H1055 | 55 | 1.20 | 48 | 850 | 170 | 135 | 203 | 10±3 | |
H1060 | 59 | 1.22 | 52 | 750 | 240 | 155 | 210 | 10±3 | |
H1863 | 63 | 1.23 | 54 | 650 | 330 | 175 | 214 | 18±3 | |
H1070 | 69 | 1.25 | 60 | 500 | 600 | 200 | 217 | 10±3 |